Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Water Absorption | 6.3 - 6.9 % | 6.3 - 6.9 % | ISO 62 |
Moisture Absorption at Equilibrium | 1.9 - 2.3 % | 1.9 - 2.3 % | 23°C/50% R.H.; ISO 62 |
Viscosity Measurement | 140 | 140 | Viscosity Number; ISO 307 |
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Melt Flow | 68 g/10 min @Load 5.00 kg, Temperature 275 °C |
68 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 185 MPa | 26800 psi | 50mm/min; ISO 527 |
Elongation at Yield | 3.5 % | 3.5 % | 50mm/min; ISO 527 |
Modulus of Elasticity | 9.50 GPa | 1380 ksi | ISO 527 |
Flexural Strength | 270 MPa | 39200 psi | ISO 178 |
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ISO 180/A |
Charpy Impact Unnotched | 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eU |
8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eA |
1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 - 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 - 13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
Melting Point | 220 °C | 428 °F | DIN 53765 |
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20,000 hr |
165 °C | 329 °F | for 50% loss of tensile strength after 5,000 hr | |
200 °C | 392 °F | ||
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
Dissipation Factor | 0.023 @Frequency 1.00e+6 Hz |
0.023 @Frequency 1.00e+6 Hz |
IEC 60250 |
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
Descriptive Properties | Value | Comments |
---|---|---|
Color | BK00564 | |
Commercial Status | North America and Europe | |
Impact Modified | No | |
Primary Processing Technique | Injection Molding |