Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.60 - 1.85 g/cc
0.0578 - 0.0668 lb/in³
Average value: 1.70 g/cc Grade Count:62
Filler Content 60.0 %
60.0 %
Average value: 60.0 % Grade Count:19
Water Absorption 0.350 - 3.60 %
0.350 - 3.60 %
Average value: 1.09 % Grade Count:27
0.800 - 1.20 %

@Temperature 70.0 - 70.0 °C
0.800 - 1.20 %

@Temperature 158 - 158 °F
Average value: 0.950 % Grade Count:4
Moisture Absorption at Equilibrium 0.700 - 1.20 %
0.700 - 1.20 %
Average value: 1.01 % Grade Count:10
Water Absorption at Saturation 3.00 - 3.70 %
3.00 - 3.70 %
Average value: 3.37 % Grade Count:11
Linear Mold Shrinkage 0.000500 - 0.0200 cm/cm
0.000500 - 0.0200 in/in
Average value: 0.00262 cm/cm Grade Count:50
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00580 cm/cm Grade Count:26
Spiral Flow 47.0 - 468 cm
18.5 - 184 in
Average value: 135 cm Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88.0 - 98.0
88.0 - 98.0
Average value: 92.8 Grade Count:3
Hardness, Rockwell R 115 - 122
115 - 122
Average value: 120 Grade Count:17
Ball Indentation Hardness 330 - 420 MPa
47900 - 60900 psi
Average value: 358 MPa Grade Count:9
Tensile Strength, Ultimate 165 - 318 MPa
23900 - 46100 psi
Average value: 245 MPa Grade Count:40
75.0 - 353.701 MPa

@Temperature -40.0 - 150 °C
10900 - 51300.1 psi

@Temperature -40.0 - 302 °F
Average value: 147 MPa Grade Count:4
130 - 130 MPa

@Temperature 130 - 175 °C
18900 - 18900 psi

@Temperature 266 - 347 °F
Average value: 147 MPa Grade Count:1
130 - 130 MPa

@Time 1.80e+7 - 7.20e+7 sec
18900 - 18900 psi

@Time 5000 - 20000 hour
Average value: 147 MPa Grade Count:1
Tensile Strength, Yield 148 - 285 MPa
21500 - 41300 psi
Average value: 223 MPa Grade Count:23
144.79 - 144.79 MPa

@Temperature 93.3 - 93.3 °C
21000 - 21000 psi

@Temperature 200 - 200 °F
Average value: 145 MPa Grade Count:1
Elongation at Break 1.00 - 4.00 %
1.00 - 4.00 %
Average value: 1.94 % Grade Count:55
1.80 - 7.50 %

@Temperature 4.44 - 150 °C
1.80 - 7.50 %

@Temperature 40.0 - 302 °F
Average value: 3.89 % Grade Count:4
Modulus of Elasticity 10.3 - 28.0 GPa
1500 - 4060 ksi
Average value: 20.3 GPa Grade Count:39
5.80 - 20.8566 GPa

@Temperature -40.0 - 150 °C
841 - 3025.05 ksi

@Temperature -40.0 - 302 °F
Average value: 11.8 GPa Grade Count:4
Flexural Yield Strength 234 - 461 MPa
33900 - 66900 psi
Average value: 361 MPa Grade Count:47
227.527 - 544.686 MPa

@Temperature -40.0 - 121 °C
33000.1 - 79000.1 psi

@Temperature -40.0 - 250 °F
Average value: 344 MPa Grade Count:2
Flexural Modulus 11.7 - 22.8 GPa
1700 - 3300 ksi
Average value: 18.1 GPa Grade Count:46
10.2732 - 19.3053 GPa

@Temperature -40.0 - 121 °C
1490.02 - 2800.04 ksi

@Temperature -40.0 - 250 °F
Average value: 14.4 GPa Grade Count:3
Izod Impact, Notched 0.950 - 7.00 J/cm
1.78 - 13.1 ft-lb/in
Average value: 2.59 J/cm Grade Count:34
7.21 - 7.68816 J/cm

@Temperature -51.1 - 149 °C
13.5 - 14.4031 ft-lb/in

@Temperature -60.0 - 300 °F
Average value: 7.51 J/cm Grade Count:2
Izod Impact, Unnotched 10.7 - 5340 J/cm
20.0 - 10000 ft-lb/in
Average value: 21.9 J/cm Grade Count:19
Izod Impact, Notched (ISO) 11.0 - 30.0 kJ/m²
5.23 - 14.3 ft-lb/in²
Average value: 15.9 kJ/m² Grade Count:5
Charpy Impact Unnotched 5.50 - 15.0 J/cm²
26.2 - 71.4 ft-lb/in²
Average value: 8.91 J/cm² Grade Count:24
6.00 - 9.70 J/cm²

@Temperature -30.0 - 30.0 °C
28.6 - 46.2 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 8.16 J/cm² Grade Count:14
Charpy Impact, Notched 1.00 - 5.40 J/cm²
4.76 - 25.7 ft-lb/in²
Average value: 1.83 J/cm² Grade Count:25
1.00 - 4.60 J/cm²

@Temperature -30.0 - 30.0 °C
4.76 - 21.9 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.45 J/cm² Grade Count:14
Dart Drop, Total Energy 7.85 - 16.4 J

@Temperature -20.0 - -20.0 °C
5.79 - 12.1 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 12.1 J Grade Count:1
7.85 - 16.4 J

@Thickness 3.18 - 3.18 mm
5.79 - 12.1 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 12.1 J Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 10.0 - 27.0 µm/m-°C
5.56 - 15.0 µin/in-°F
Average value: 20.5 µm/m-°C Grade Count:25
CTE, linear, Transverse to Flow 40.0 - 55.0 µm/m-°C
22.2 - 30.6 µin/in-°F
Average value: 44.3 µm/m-°C Grade Count:7
Thermal Conductivity 0.300 - 0.548 W/m-K
2.08 - 3.80 BTU-in/hr-ft²-°F
Average value: 0.424 W/m-K Grade Count:4
Melting Point 220 - 325 °C
428 - 617 °F
Average value: 267 °C Grade Count:25
Maximum Service Temperature, Air 135 - 250 °C
275 - 482 °F
Average value: 186 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 220 - 260 °C
428 - 500 °F
Average value: 255 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 210 - 300 °C
410 - 572 °F
Average value: 253 °C Grade Count:51
Deflection Temperature at 8.0 MPa 180 - 250 °C
356 - 482 °F
Average value: 226 °C Grade Count:8
Vicat Softening Point 240 - 255 °C
464 - 491 °F
Average value: 251 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:24
Glow Wire Test 650 °C
1200 °F
Average value: 650 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cm
1.00e+9 - 1.00e+16 ohm-cm
Average value: 4.47e+14 ohm-cm Grade Count:24
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 5.11e+14 ohm Grade Count:20
Dielectric Strength 19.7 - 35.0 kV/mm
500 - 889 kV/in
Average value: 24.6 kV/mm Grade Count:18
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:9