Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2033THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 148 - 285 MPa | 21500 - 41300 psi | Average value: 223 MPa Grade Count:23 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF30 HF L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: Lubricated and High FlowAppearance: BlackInformation provi.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 TL20 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE Lubricant (20%) Features: LubricatedAppearance: BlackInformation provided.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | Annealed |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Techmer ES HiFill® PEI GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 148 MPa | 21400 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 148 MPa @Strain 0.200 % |
21500 psi @Strain 0.200 % |
Typical; Annealed |
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 148 MPa | 21500 psi | ASTM D638 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |