Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 55.0 µm/m-°C | 22.2 - 30.6 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature -40.0 - 150 °C |
22.2 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | TMA |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 XL PET-GF35 35% Glass Reinforced, Low Outgassing |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65 Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade PBT-GF50Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
Arlon AD410 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X682 Novolac Phenolic Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 59.3 µm/m-°C Grade Count:21 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 120 µm/m-°C | 22.2 - 66.7 µin/in-°F | Average value: 80.8 µm/m-°C Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 85.0 µm/m-°C | 22.2 - 47.2 µin/in-°F | Average value: 61.8 µm/m-°C Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |