Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.0448 - 145 MPa | 6.50 - 21000 psi | Average value: 6.06 MPa Grade Count:110 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Yield | 144.79 - 144.79 MPa @Temperature 93.3 - 93.3 °C |
21000 - 21000 psi @Temperature 200 - 200 °F |
Average value: 145 MPa Grade Count:1 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Yield | 46.0 - 145 MPa | 6670 - 21000 psi | Average value: 90.2 MPa Grade Count:18 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 144.79 - 144.79 MPa @Temperature 93.3 - 93.3 °C |
21000 - 21000 psi @Temperature 200 - 200 °F |
Average value: 145 MPa Grade Count:1 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Tensile Strength, Yield | 55.8 - 145 MPa | 8100 - 21000 psi | Average value: 83.2 MPa Grade Count:10 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Yield | 91.0 - 145 MPa | 13200 - 21000 psi | Average value: 114 MPa Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |