Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific) High flow Ultem blends for thin wall application |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 0.000 °C |
1.78 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature -30.0 °C |
1.78 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ISO 180 |
Stir SpA RF 1000A (PVC) Application: Extrusion shock resistant profiles for windowsInformation provided by STIR SpA |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough RZ309G18 Polycarbonate, 18% Glass Fiber 18% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate 10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.17 mm |
1.78 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.17 mm |
1.78 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |