Polymer Property : Charpy Impact, Notched = 25.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 - 5.40 J/cm²
4.76 - 25.7 ft-lb/in²
Average value: 1.83 J/cm² Grade Count:25
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Charpy Impact, Notched 0.210 - 5.40 J/cm²
0.999 - 25.7 ft-lb/in²
Average value: 1.36 J/cm² Grade Count:26
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.150 - 5.40 J/cm²
0.714 - 25.7 ft-lb/in²
Average value: 2.85 J/cm² Grade Count:12
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..