Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+9 - 1.00e+15 ohm-cm @Temperature 125 - 275 °C |
1.00e+9 - 1.00e+15 ohm-cm @Temperature 257 - 527 °F |
Average value: 5.00e+14 ohm-cm Grade Count:8 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm | 1.00e+9 - 1.00e+17 ohm-cm | Average value: 7.17e+15 ohm-cm Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 2.60e+15 ohm-cm Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 5.32e+15 ohm-cm Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 6.46e+15 ohm-cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 7.42e+14 ohm-cm Grade Count:41 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 8.66e+14 ohm-cm Grade Count:24 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+15 ohm-cm | 1.00e+9 - 1.00e+15 ohm-cm | Average value: 2.37e+14 ohm-cm Grade Count:72 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+15 ohm-cm | 1.00e+9 - 1.00e+15 ohm-cm | Average value: 4.88e+14 ohm-cm Grade Count:28 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 4.47e+14 ohm-cm Grade Count:24 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm | 1.00e+9 - 1.00e+17 ohm-cm | Average value: 2.75e+15 ohm-cm Grade Count:44 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Sapco Partially Stabilized TZP Zirconia (YSZ) Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm @Temperature 500 °C |
1.00e+9 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek Zirconia-Toughened Alumina, ZTA Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm | 1.00e+9 - 1.00e+17 ohm-cm | Average value: 1.98e+16 ohm-cm Grade Count:15 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+18 ohm-cm | 1.00e+9 - 1.00e+18 ohm-cm | Average value: 1.28e+16 ohm-cm Grade Count:96 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+9 - 3.20e+12 ohm-cm @Temperature 150 - 150 °C |
1.00e+9 - 3.20e+12 ohm-cm @Temperature 302 - 302 °F |
Average value: 1.03e+12 ohm-cm Grade Count:8 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
CENTROPLAST CENTROSOL LF Acrylonitrile butadiene Styrene copolymer conductive CENTROSOL LF ABS has high rigidity and hardness even at low temperatures. It is permanently conductive and is used in support components for the semi-conductor industry.Information provided by CENT.. |
|||
Electrical Resistivity | 1.00e+9 - 2.30e+17 ohm-cm | 1.00e+9 - 2.30e+17 ohm-cm | Average value: 4.72e+16 ohm-cm Grade Count:59 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |