Polymer Property : Charpy Impact, Notched = 4.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 - 4.60 J/cm²

@Temperature -30.0 - 30.0 °C
4.76 - 21.9 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.45 J/cm² Grade Count:14
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..