Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 191 - 255 °C | 376 - 491 °F | Average value: 207 °C Grade Count:22 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Vicat Softening Point | 225 - 255 °C | 437 - 491 °F | Average value: 240 °C Grade Count:4 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Vicat Softening Point | 225 - 255 °C | 437 - 491 °F | Average value: 241 °C Grade Count:25 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Vicat Softening Point | 240 - 255 °C | 464 - 491 °F | Average value: 251 °C Grade Count:4 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Vicat Softening Point | 230 - 255 °C | 446 - 491 °F | Average value: 248 °C Grade Count:5 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Vicat Softening Point | 230 - 255 °C | 446 - 491 °F | Average value: 246 °C Grade Count:7 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Vicat Softening Point | 200 - 255 °C | 392 - 491 °F | Average value: 241 °C Grade Count:13 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Vicat Softening Point | 205 - 255 °C | 401 - 491 °F | Average value: 232 °C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |