Mechanical Properties Metric English Comments
Tensile Strength, Yield 148 - 285 MPa
21500 - 41300 psi
Average value: 223 MPa Grade Count:23
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..