Polymer Property : Charpy Impact Unnotched = 28.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179-1
Polycasa XT 610 PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® S650FR BK851 PBT  (Unverified Data**)
Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 20-7868 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 50-7216 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East)
Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized
A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30
Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65
Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30
Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15
Information provided by EMS Grivory
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66  (Unverified Data**)
30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin
15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Celanese Celstran® PA66-GF50-02 P11/14 Nylon 66, 50% Glass Reinforced
Material code according to ISO 1043-1: PA66Information provided by Celanese
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Hostaform® C 9021 TF POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50
Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Celanese Celstran® +PP-GF60-04CN15/10 PP, 60% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese