Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 7.68816 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.42712 - 7.68816 J/cm

@Temperature -40.0 - -18.0 °C
0.80017 - 14.4031 ft-lb/in

@Temperature -40.0 - -0.400 °F
Average value: 1.66 J/cm Grade Count:31
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 7.21 - 7.68816 J/cm

@Temperature -51.1 - 149 °C
13.5 - 14.4031 ft-lb/in

@Temperature -60.0 - 300 °F
Average value: 7.51 J/cm Grade Count:2
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Copyright © lookpolymers.com All Rights Reserved