Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.80 - 20.8566 GPa @Temperature -40.0 - 150 °C |
841 - 3025.05 ksi @Temperature -40.0 - 302 °F |
Average value: 11.8 GPa Grade Count:4 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | ISO 527-2 |
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 V30 Nylon 66, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 ZV30 Nylon 66, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | ISO 527-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | ISO 527-1/-2 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Modulus of Elasticity | 5.80 GPa | 841 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Modulus of Elasticity | 5.80 - 20.8 GPa | 841 - 3020 ksi | Average value: 10.4 GPa Grade Count:16 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |