Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | >= 10.7 J/cm | >= 20.0 ft-lb/in | ASTM D256 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 16.4 J/cm Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Unnotched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® C-40 40% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 - 42.7 J/cm | 20.0 - 80.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |