Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.11 - 1.82 g/cc
0.0401 - 0.0658 lb/in³
Average value: 1.38 g/cc Grade Count:811
1.12 - 1.40 g/cc

@Temperature 250 - 295 °C
0.0405 - 0.0506 lb/in³

@Temperature 482 - 563 °F
Average value: 1.23 g/cc Grade Count:11
Filler Content 25.0 - 35.0 %
25.0 - 35.0 %
Average value: 29.8 % Grade Count:115
Water Absorption 0.200 - 6.90 %
0.200 - 6.90 %
Average value: 2.03 % Grade Count:437
1.55 - 2.20 %

@Temperature 70.0 - 70.0 °C
1.55 - 2.20 %

@Temperature 158 - 158 °F
Average value: 1.95 % Grade Count:5
Moisture Absorption at Equilibrium 0.170 - 5.70 %
0.170 - 5.70 %
Average value: 1.78 % Grade Count:230
Water Absorption at Saturation 0.800 - 9.00 %
0.800 - 9.00 %
Average value: 5.41 % Grade Count:88
Additive Loading 25.0 - 33.0 %
25.0 - 33.0 %
Average value: 29.8 % Grade Count:8
Viscosity 20.0 - 500 cP

@Temperature 270 - 300 °C
20.0 - 500 cP

@Temperature 518 - 572 °F
Average value: 141 cP Grade Count:8
20.0 - 500 cP

@Shear Rate 10.0 - 1000 1/s
20.0 - 500 cP

@Shear Rate 10.0 - 1000 1/s
Average value: 141 cP Grade Count:8
Viscosity Test 127 - 210 cm³/g
127 - 210 cm³/g
Average value: 147 cm³/g Grade Count:23
Maximum Moisture Content 0.0900 - 0.100
0.0900 - 0.100
Average value: 0.0929 Grade Count:7
Linear Mold Shrinkage 0.000400 - 0.0550 cm/cm
0.000400 - 0.0550 in/in
Average value: 0.00459 cm/cm Grade Count:661
Linear Mold Shrinkage, Transverse 0.000500 - 0.0190 cm/cm
0.000500 - 0.0190 in/in
Average value: 0.00923 cm/cm Grade Count:257
Melt Flow 1.00 - 198 g/10 min
1.00 - 198 g/10 min
Average value: 31.9 g/10 min Grade Count:71
Spiral Flow 69.0 - 757 cm
27.2 - 298 in
Average value: 137 cm Grade Count:14
Mechanical Properties Metric English Comments
Hardness, Rockwell L 108 - 114
108 - 114
Average value: 111 Grade Count:18
Hardness, Rockwell M 58.0 - 104
58.0 - 104
Average value: 88.8 Grade Count:56
Hardness, Rockwell R 85.0 - 124
85.0 - 124
Average value: 116 Grade Count:178
Hardness, Shore D 77.0 - 90.0
77.0 - 90.0
Average value: 83.6 Grade Count:10
Ball Indentation Hardness 125 - 280 MPa
18100 - 40600 psi
Average value: 213 MPa Grade Count:40
Tensile Strength, Ultimate 30.0 - 215 MPa
4350 - 31200 psi
Average value: 149 MPa Grade Count:581
35.0 - 235 MPa

@Temperature -40.0 - 150 °C
5080 - 34100 psi

@Temperature -40.0 - 302 °F
Average value: 88.6 MPa Grade Count:14
90.0 - 105 MPa

@Temperature 130 - 175 °C
13100 - 15200 psi

@Temperature 266 - 347 °F
Average value: 88.6 MPa Grade Count:5
90.0 - 105 MPa

@Time 1.80e+7 - 7.20e+7 sec
13100 - 15200 psi

@Time 5000 - 20000 hour
Average value: 88.6 MPa Grade Count:5
25.0 - 215 MPa

@Strain 1.00 - 10.0 %
3630 - 31200 psi

@Strain 1.00 - 10.0 %
Average value: 88.6 MPa Grade Count:5
25.0 - 215 MPa

@Temperature -40.0 - 150 °C
3630 - 31200 psi

@Temperature -40.0 - 302 °F
Average value: 88.6 MPa Grade Count:5
Tensile Strength, Yield 18.8 - 290 MPa
2730 - 42100 psi
Average value: 155 MPa Grade Count:251
231 - 240 MPa

@Temperature -40.0 - -40.0 °C
33500 - 34800 psi

@Temperature -40.0 - -40.0 °F
Average value: 236 MPa Grade Count:2
Elongation at Break 1.00 - 200 %
1.00 - 200 %
Average value: 4.04 % Grade Count:717
2.40 - 6.80 %

@Temperature 4.44 - 150 °C
2.40 - 6.80 %

@Temperature 40.0 - 302 °F
Average value: 4.99 % Grade Count:12
Elongation at Yield 2.00 - 11.0 %
2.00 - 11.0 %
Average value: 4.12 % Grade Count:72
3.50 - 6.00 %

@Temperature 60.0 - 150 °C
3.50 - 6.00 %

@Temperature 140 - 302 °F
Average value: 4.68 % Grade Count:6
Modulus of Elasticity 1.00 - 15.0 GPa
145 - 2180 ksi
Average value: 8.43 GPa Grade Count:471
0.220 - 11.05 GPa

@Temperature -100 - 250 °C
31.9 - 1603 ksi

@Temperature -148 - 482 °F
Average value: 5.50 GPa Grade Count:19
Flexural Yield Strength 65.0 - 325 MPa
9430 - 47100 psi
Average value: 226 MPa Grade Count:595
100 - 315 MPa

@Temperature -40.0 - 121 °C
14500 - 45700 psi

@Temperature -40.0 - 250 °F
Average value: 184 MPa Grade Count:9
Flexural Modulus 0.758 - 13.5 GPa
110 - 1960 ksi
Average value: 7.83 GPa Grade Count:663
3.10 - 10.8 GPa

@Temperature -40.0 - 121 °C
450 - 1570 ksi

@Temperature -40.0 - 250 °F
Average value: 5.75 GPa Grade Count:11
Compressive Yield Strength 28.0 - 241 MPa
4060 - 35000 psi
Average value: 145 MPa Grade Count:18
Poissons Ratio 0.350 - 0.420
0.350 - 0.420
Average value: 0.389 Grade Count:17
Fatigue Strength >= 47.7 MPa

@Temperature 80.0 - 120 °C
>= 6920 psi

@Temperature 176 - 248 °F
Average value: 59.1 MPa Grade Count:2
>= 47.7 MPa

@Time 7200 - 817000 sec
>= 6920 psi

@Time 2.00 - 227 hour
Average value: 59.1 MPa Grade Count:2
Shear Modulus 1.46 - 3.90 GPa
212 - 566 ksi
Average value: 2.45 GPa Grade Count:13
>= 0.209 GPa

@Temperature -50.0 - 250 °C
>= 30.3 ksi

@Temperature -58.0 - 482 °F
Average value: 1.09 GPa Grade Count:9
Shear Strength 50.0 - 90.0 MPa
7250 - 13100 psi
Average value: 76.8 MPa Grade Count:26
Izod Impact, Notched 0.481 - 75.0 J/cm
0.900 - 141 ft-lb/in
Average value: 1.37 J/cm Grade Count:363
0.500 - 3.84408 J/cm

@Temperature -40.0 - 149 °C
0.937 - 7.20154 ft-lb/in

@Temperature -40.0 - 300 °F
Average value: 1.34 J/cm Grade Count:3
0.64068 - 2.24238 J/cm

@Temperature -40.0 - 72.8 °C
1.2003 - 4.20090 ft-lb/in

@Temperature -40.0 - 163 °F
Average value: 1.34 J/cm Grade Count:5
0.64068 - 2.24238 J/cm

@Thickness 3.17 - 3.17 mm
1.2003 - 4.20090 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.34 J/cm Grade Count:5
Izod Impact, Unnotched 1.07 J/cm - NB
2.00 ft-lb/in - NB
Average value: 8.19 J/cm Grade Count:68
Izod Impact, Notched (ISO) 2.50 - 95.0 kJ/m²
1.19 - 45.2 ft-lb/in²
Average value: 13.0 kJ/m² Grade Count:240
5.00 - 19.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.38 - 9.04 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 10.2 kJ/m² Grade Count:111
Izod Impact, Unnotched (ISO) 7.00 - 90.0 kJ/m²
3.33 - 42.8 ft-lb/in²
Average value: 60.9 kJ/m² Grade Count:31
Users viewing this material also viewed the following: