Polymer Property : Density = 0.0401 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Nylene® 826 Nylon Copolymer
Dry as molded. Nylene 826 is a special nylon copolymer suitable for both blown and cast film co-extrusion. Nylene 826 has a lower melt point and is less crystalline than standard nylon 6 resins. In..
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792-60T
Rotuba 860MH 686.4 Ethyl Cellulose
Data provided by the manufacturer.
Density 1.11 g/cc
0.0401 lb/in³
NCMT Method
NCMT NanoPAC™ G1550S High Performance Polypropylene Nanocomposite
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Polykemi AB SCANAMID 66 A32^E Nylon 66, Modified
Information provided by Polykemi AB
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder  (discontinued **)
Data provided by PolyOne.
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Density 1.11 g/cc

@Temperature 25.0 °C
0.0401 lb/in³

@Temperature 77.0 °F
DSM Somos® 8120 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1
Kraiburg TPE For-Tec E OC7OAN Thermoplastic Elastomer, Adhesion to PA
The AD/PAX/MR Series is recommended for two-component-seals in electronic applications and soft touch grips and handles of machine tools. The material provides an excellent resistance to skin oils, ..
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® TF5BNB Thermoplastic Elastomer, natural
Typical Markets / Application Sectors:Packaging FoodPersonal Care & Baby CareStationariesElectric Household ApplianceHousehold goodsApplication Examples:Anti-slip elementsFunctional elementsHandlesD..
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime..
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform..
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
PlastxWorld CEVIAN® E80 ABS
Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Unitika CX-2500 PA6, Conditioned
Transparent nylonInformation provided by Unitika Ltd.
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Unitika CX-2500 PA6, Dry
Transparent nylonInformation provided by Unitika Ltd.
Density 1.11 g/cc
0.0401 lb/in³
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by..
Density 1.11 g/cc
0.0401 lb/in³
Covestro Bayblend® KU 1-1446 Polycarbonate/ABS Blend
Good cold impact strength and fuel resistance.Applications: Automotive industry (interior and body parts).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated fr..
Density 1.11 g/cc
0.0401 lb/in³
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. ..
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Ashley Polymers Ashlene® 526LD Nylon 66
Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Aclo Accutech Polypropylene Copolymer CP0436G5M25CL Glass/Mineral Reinforced Coupled
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® K TF7BNA Thermoplastic Elastomer, General purpose  (Unverified Data**)
Application Examples:SealsHandlesConsumer articlesMaterial Advantages:Extremely flexibleEasy to colorBfR, FDA, 2002/72/EC and EN 71/3 compliantGood physical propertiesSmooth surfaceAdhesion to PPOpe..
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® K TF8BNA Thermoplastic Elastomer, General purpose  (Unverified Data**)
Application Examples:SealsHandlesConsumer articlesMaterial Advantages:Extremely flexibleEasy to colorBfR, FDA, 2002/72/EC and EN 71/3 compliantGood physical propertiesSmooth surfaceAdhesion to PPOpe..
Density 1.11 g/cc
0.0401 lb/in³
ASTM A792
PlastxWorld Veroplas PA2002MI Nylon 6
general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc.
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® K TC7HAA Natural TPE  (Unverified Data**)
Adhesion to POM (Hostaform®, Duracon, Celcon)Patented system for TPE-S and POMEasy processabilityBroad service temperature rangeTypical Applications: Hard/soft applications with POM:SealingOver mol..
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.