Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.84 - 10.8 GPa | 992 - 1570 ksi | Average value: 9.34 GPa Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Flexural Modulus | 3.10 - 10.8 GPa @Temperature -40.0 - 121 °C |
450 - 1570 ksi @Temperature -40.0 - 250 °F |
Average value: 5.75 GPa Grade Count:11 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Modulus | 10.2 - 10.8 GPa | 1480 - 1570 ksi | ASTM D790M |
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi.. |
|||
Flexural Modulus | 9.00 - 10.8 GPa | 1310 - 1570 ksi | Average value: 9.67 GPa Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |