Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 100 - 315 MPa @Temperature -40.0 - 121 °C |
14500 - 45700 psi @Temperature -40.0 - 250 °F |
Average value: 184 MPa Grade Count:9 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |