Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²
1.19 - 5.71 ft-lb/in²
Average value: 6.75 kJ/m² Grade Count:6
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -40.0 °C
1.19 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin  (discontinued **)
Thermoplastic Polyolefin, High Stiffness, Talc-FilledApplications: Automotive InteriorsConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.9-1.1%Drying conditionsTemperature: 80-100°CTim..
Izod Impact, Notched (ISO) 2.50 - 47.0 kJ/m²
1.19 - 22.4 ft-lb/in²
Average value: 8.19 kJ/m² Grade Count:104
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²
1.19 - 5.71 ft-lb/in²
Average value: 5.29 kJ/m² Grade Count:33
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched (ISO) 2.50 - 107 kJ/m²
1.19 - 50.9 ft-lb/in²
Average value: 9.85 kJ/m² Grade Count:38
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 2.50 - 85.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.19 - 40.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 21.0 kJ/m² Grade Count:5
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Izod Impact, Notched (ISO) 2.50 - 95.0 kJ/m²
1.19 - 45.2 ft-lb/in²
Average value: 13.0 kJ/m² Grade Count:240
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Notched (ISO) 2.50 - 47.0 kJ/m²
1.19 - 22.4 ft-lb/in²
Average value: 14.3 kJ/m² Grade Count:111
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Type 1, Notch A; ISO 180
LyondellBasell Moplen HP400N Polypropylene Homopolymer
Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Sample Type A; ISO 180:2000
Global EPP PET SL PET + Solid Lubricant
PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani..
Izod Impact, Notched (ISO) >= 2.50 kJ/m²
>= 1.19 ft-lb/in²
ISO 180-1A
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry
Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) >= 2.50 kJ/m²
>= 1.19 ft-lb/in²
ISO 180-1A
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ASTM D256
Tipco Tipcolene® FPT 40 - 40% Talc Reinforced Polypropylene Homopolymer Compound
40% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180-93
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66
Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman.
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 179
Total PPH 10060 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 10060 homopolymer. PPH 10060 is characterized by high fluidity and is particularly suitable for injection molding applications. The material provides a good balance betwe..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180
Total PPH 11012 Polypropylene Homopolymer, Injection Molding
Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed ..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM..
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -40.0 °C
1.19 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 BK010 is a 30% mineral reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Pe..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead
Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast.
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180/1A
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²
1.19 - 47600 ft-lb/in²
Average value: 14.6 kJ/m² Grade Count:33
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu..
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²
1.19 - 47600 ft-lb/in²
Average value: 6.56 kJ/m² Grade Count:10
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Copyright © lookpolymers.com All Rights Reserved