Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.64068 - 2.24238 J/cm @Temperature -40.0 - 72.8 °C |
1.2003 - 4.20090 ft-lb/in @Temperature -40.0 - 163 °F |
Average value: 1.34 J/cm Grade Count:5 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched | 0.64068 - 2.24238 J/cm @Thickness 3.17 - 3.17 mm |
1.2003 - 4.20090 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.34 J/cm Grade Count:5 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |