Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm
0.00100 - 0.0190 in/in
Average value: 0.00861 cm/cm Grade Count:23
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage, Transverse 0.00600 - 0.0190 cm/cm
0.00600 - 0.0190 in/in
Average value: 0.0130 cm/cm Grade Count:5
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0190 cm/cm
0.00400 - 0.0190 in/in
Average value: 0.0104 cm/cm Grade Count:14
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Linear Mold Shrinkage, Transverse 0.0110 - 0.0190 cm/cm
0.0110 - 0.0190 in/in
Average value: 0.0162 cm/cm Grade Count:26
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.000500 - 0.0190 cm/cm
0.000500 - 0.0190 in/in
Average value: 0.00923 cm/cm Grade Count:257
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm
0.00100 - 0.0190 in/in
Average value: 0.0127 cm/cm Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..