Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | >= 47.7 MPa @Temperature 80.0 - 120 °C |
>= 6920 psi @Temperature 176 - 248 °F |
Average value: 59.1 MPa Grade Count:2 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Fatigue Strength | >= 47.7 MPa @Time 7200 - 817000 sec |
>= 6920 psi @Time 2.00 - 227 hour |
Average value: 59.1 MPa Grade Count:2 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |