Mechanical Properties Metric English Comments
Shear Strength 50.0 - 65.0 MPa
7250 - 9430 psi
Average value: 58.0 MPa Grade Count:3
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Shear Strength 50.0 - 76.5 MPa
7250 - 11100 psi
Average value: 61.7 MPa Grade Count:5
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Shear Strength 50.0 - 90.0 MPa
7250 - 13100 psi
Average value: 76.8 MPa Grade Count:26
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Shear Strength 50.0 MPa
7250 psi
0º, Short Beam
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 300 g/m2
Information provided by HexCel
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Sheets
Description: Exclusively for mechanical applications. Impact-resistant. Resistant to mechanical wear and noise-reducing. The graphite content causes low friction. Well suited for parts where there a..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MFP G Phenolic, Cotton/synthetic Fabric Reinforcement, Black, Sheets
Description: Exclusively for mechanical applications. The combination of cotton/synthetic reinforcement and a graphite-modified resin results in a material with low friction and especially high wear..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Shear Strength 50.0 - 65.0 MPa
7250 - 9430 psi
IS 867-1963
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Shear Strength 50.0 - 65.0 MPa
7250 - 9430 psi
IS 867-1963
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..