Material Notes:
Applications: closures, thin wall containers, and excellent transparency.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Tensile Strength, Yield 29.0 MPa
4210 psi
50mm/min; ISO 527-2
Elongation at Yield 11 %
11 %
50mm/min; ISO 527-2
Tensile Modulus 1.15 GPa
167 ksi
1mm/min; ISO 527-3
Charpy Impact, Notched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high