Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66GF33BK Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66MI40N Nylon 66, 40% Mineral Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PPCM15BK Copolymer PP Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | Average value: 1.74 J/cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | 1.07 - 6.94 J/cm | 2.00 - 13.0 ft-lb/in | Average value: 3.89 J/cm Grade Count:35 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | Average value: 1.90 J/cm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched | 1.07 J/cm - NB | 2.00 ft-lb/in - NB | Average value: 8.19 J/cm Grade Count:68 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Spartech SP-2010 HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | Notch Status Unknown |
Goodfellow Manganin® Copper Resistance Alloy Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In.. |
|||
Izod Impact, Unnotched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 1.07 - 7.29 J/cm | 2.00 - 13.7 ft-lb/in | Average value: 4.58 J/cm Grade Count:28 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 1.07 - 4.30 J/cm | 2.00 - 8.06 ft-lb/in | Average value: 2.12 J/cm Grade Count:30 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Izod Impact, Unnotched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Spartech Solarex® K High Heat Weatherable Copolyester Sign Grade Sheet Information provided by Spartech. |
|||
Izod Impact, Unnotched | 1.07 - 11.2 J/cm | 2.00 - 21.0 ft-lb/in | Average value: 3.74 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 1.07 - 6.41 J/cm | 2.00 - 12.0 ft-lb/in | Average value: 3.51 J/cm Grade Count:8 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |