Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 69.0 - 757 cm | 27.2 - 298 in | Average value: 137 cm Grade Count:14 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |