Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000400 - 0.00300 cm/cm | 0.000400 - 0.00300 in/in | Average value: 0.00157 cm/cm Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0140 cm/cm | 0.000400 - 0.0140 in/in | Average value: 0.00826 cm/cm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0550 cm/cm | 0.000400 - 0.0550 in/in | Average value: 0.00459 cm/cm Grade Count:661 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0190 cm/cm | 0.000400 - 0.0190 in/in | Average value: 0.0116 cm/cm Grade Count:93 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0420 cm/cm | 0.000400 - 0.0420 in/in | Average value: 0.0148 cm/cm Grade Count:262 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |