Material Notes:
Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be formed inside this material for water cooling.Information provided by M Cubed Technologies, Inc.
Physical Properties Metric English Comments
Density 3.13 g/cc
0.113 lb/in³
ASTM C135
Mechanical Properties Metric English Comments
Knoop Microhardness 1400

@Load 2.00 kg
1400

@Load 4.41 lb
kg/mm2; ASTM C1326
Modulus of Elasticity 390 GPa
56600 ksi
ASTM E494
Flexural Strength 250 MPa
36300 psi
ASTM C1161
Poissons Ratio 0.19
0.19
ASTM E494
Fracture Toughness 4.80 MPa-m½
4.37 ksi-in½
ASTM C1421
Shear Modulus 164 GPa
23800 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 25.0 - 100 °C
1.67 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
ASTM E1461
Descriptive Properties Value Comments
Matrix Ti-Si
Particle Reinforcement SiC
Vol. % Reinforcement 80