Mechanical Properties Metric English Comments
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL A63 HH-TFGV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL A63 HS-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL B63 S Nylon 6 for injection molding
Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL B63 D-S 5 Nylon 6., std. viscosity for injection molding
Nylon 6., std. viscosity for injection molding, permanently flexible, dry impact resistant for high quality dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039-1
Nilit FRIANYL B63 ND Nylon 6
Nylon 6, low viscosity, permanently flexible, dry impact resistant (dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 125 - 280 MPa
18100 - 40600 psi
Average value: 213 MPa Grade Count:40
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Ball Indentation Hardness 125 MPa
18100 psi
HB 961/30; ISO 2039-1
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Ball Indentation Hardness 125 MPa
18100 psi
ISO 2039
GEHR Plastics POM-C Acetal
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be..
Ball Indentation Hardness 125 MPa
18100 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 125 MPa
18100 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30
Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid..
Ball Indentation Hardness 125 MPa
18100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSZ 1 PA666
Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha..
Ball Indentation Hardness 125 MPa
18100 psi
358/30; ISO 2039-1
BASF Ultraform H 4320 Q600 POM
Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency ..