Ball Indentation Hardness 125 - 280 MPa
18100 - 40600 psi
Average value: 213 MPa Grade Count:40
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..