Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.209 GPa @Temperature -50.0 - 250 °C |
>= 30.3 ksi @Temperature -58.0 - 482 °F |
Average value: 1.09 GPa Grade Count:9 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |