| Lanxess Durethan® A 30 H2.0 901510 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® A 30 S 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® AC 30 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber | Nylon 66, 10% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers | Nylon 66, 20% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber | Nylon 66, Heat Stabilized | Durethan® | 
            
        | Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber | Nylon 66, 50% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers | Nylon 66, 50% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber | Nylon 66, 20% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66 | Nylon 66, Impact Grade | Durethan® | 
            
        | Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber | Nylon 66, Glass Fiber Filled, Flame Retardant | Durethan® | 
            
        | Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 | Nylon 66, Unreinforced, Flame Retardant | Durethan® | 
            
        | Lanxess Durethan® DP A 32 901510 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber | Nylon 66, Glass Fiber Filled, Flame Retardant | Durethan® | 
            
        | Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber | Nylon 66, 30% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® A 30 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® A 30 H3.0 000000 Nylon 66 | Nylon 66, Heat Stabilized | Durethan® | 
            
        | Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant | Nylon 66, Unreinforced, Flame Retardant | Durethan® | 
            
        | Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber | Nylon 66, 20% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber | Nylon 66, 20% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced | Nylon 66, 40% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber | Nylon 66, 50% Glass Fiber Filled | Durethan® | 
            
        | Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber | Nylon 66, Glass Fiber Filled, Flame Retardant | Durethan® | 
            
        | Lanxess Durethan® DP 2801 000000 Nylon 66 | Nylon 66, Unreinforced | Durethan® | 
            
        | Lanxess Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber | Nylon 66, 40% Glass Fiber Filled | Durethan® |