| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
| Water Absorption | 5.5 % | 5.5 % | Test Sim. to ISO 62 |
| Moisture Absorption at Equilibrium | 2.0 % | 2.0 % | 23°C/50% R.H.; Test Sim. to ISO 62 |
| Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 280 °C |
14 g/10 min @Load 11.0 lb, Temperature 536 °F |
Estimated using room temperature density; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 120 MPa | 17400 psi | Conditioned; ISO 527-1/-2 |
| 180 MPa | 26100 psi | ISO 527-1/-2 | |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1/-2 |
| 8.0 % | 8.0 % | Conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 6.10 GPa | 885 ksi | Conditioned; ISO 527-1/-2 |
| 9.50 GPa | 1380 ksi | ISO 527-1/-2 | |
| Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU | |
| 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU | |
| 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eA | |
| 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
| 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 125 °C | 257 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
IEC 60695-11-10 | |
| Oxygen Index | 25 % | 25 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; IEC 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 | |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.6 @Frequency 1.00e+6 Hz |
3.6 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 4.0 @Frequency 100 Hz |
4.0 @Frequency 100 Hz |
IEC 60250 | |
| 4.5 @Frequency 1.00e+6 Hz |
4.5 @Frequency 1.00e+6 Hz |
Conditioned; IEC 60250 | |
| 12 @Frequency 100 Hz |
12 @Frequency 100 Hz |
Conditioned; IEC 60250 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; IEC 60243-1 |
| 35.0 kV/mm | 889 kV/in | IEC 60243-1 | |
| Dissipation Factor | 0.0080 @Frequency 100 Hz |
0.0080 @Frequency 100 Hz |
IEC 60250 |
| 0.016 @Frequency 1.00e+6 Hz |
0.016 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| 0.090 @Frequency 1.00e+6 Hz |
0.090 @Frequency 1.00e+6 Hz |
Conditioned; IEC 60250 | |
| 0.30 @Frequency 100 Hz |
0.30 @Frequency 100 Hz |
Conditioned; IEC 60250 | |
| Comparative Tracking Index | 450 V | 450 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets | |
| ISO Shortname | ISO 1874-PA 66,MHWR,18-100,GF30 | |
| Processing | Injection molding | |
| Region | Asia Pacific | |
| Europe | ||
| Near East/Africa | ||
| North America | ||
| South and Central America |