Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-freeze solutions at elevated temperatures. This product is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher heat distortion temperature, resistance to creep and better dimensional stability when compared with unreinforced PA66. These products have good chemical resistance to a broad range of chemicals including gasoline, hydraulic fluids and most solvents. Vydyne R533H NT is heat-stabilized to minimize oxidative degradation of the polymer when exposed to elevated temperatures in service. This product provides improved retention of physical properties under exposure to long-term heat. Also, Vydyne R533H NT has excellent knit-line strength and fatigue resistance, which is essential for cycle testing with anti-freeze solutions. Typical Applications/End Uses: Vydyne R533H NT has been used for several under-the-hood automotive applications, motor housings for power tools and garden appliance. This resin has also been used in miscellaneous brackets, gears and clips that require high rigidity and strength. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 33% Filler by WeightAdditive:Heat StabilizerLubricant Features: Good FlowGood Mold ReleaseHeat Stabilized High RigidityHigh StrengthHydrolysis Resistant Lubricated Uses: Automotive Under the HoodGearsHousingsPower/Other Tools Appearance: NaturalForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption 0.80 %
<br>@Time 86400 sec
0.80 %
<br>@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
<br>@Diameter 2.00 mm
0.0040 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
<br>@Diameter 2.00 mm
0.0090 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 205 MPa
29700 psi
ISO 527-2
Elongation at Break 3.0 %
3.0 %
ISO 527-2
Tensile Modulus 10.6 GPa
1540 ksi
ISO 527-2
Flexural Strength 290 MPa
42100 psi
ISO 178
Flexural Modulus 10.2 GPa
1480 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
12.0 kJ/m²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature -30.0 °C
33.3 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
1.10 J/cm²
<br>@Temperature 23.0 °C
5.23 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 2.10 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
1.17 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 11.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
6.11 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Unannealed; ISO 75-2/A
UL RTI, Electrical 140 °C
<br>@Thickness 0.750 mm
284 °F
<br>@Thickness 0.0295 in
UL 746
140 °C
<br>@Thickness 1.50 mm
284 °F
<br>@Thickness 0.0591 in
UL 746
140 °C
<br>@Thickness 3.00 mm
284 °F
<br>@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact 125 °C
<br>@Thickness 0.750 mm
257 °F
<br>@Thickness 0.0295 in
UL 746
125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL 746
125 °C
<br>@Thickness 3.00 mm
257 °F
<br>@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 140 °C
<br>@Thickness 0.750 mm
284 °F
<br>@Thickness 0.0295 in
UL 746
140 °C
<br>@Thickness 1.50 mm
284 °F
<br>@Thickness 0.0591 in
UL 746
140 °C
<br>@Thickness 3.00 mm
284 °F
<br>@Thickness 0.118 in
UL 746
Flammability, UL94 HB
<br>@Thickness 0.750 mm
HB
<br>@Thickness 0.0295 in
HB
<br>@Thickness 1.50 mm
HB
<br>@Thickness 0.0591 in
HB
<br>@Thickness 3.00 mm
HB
<br>@Thickness 0.118 in
Glow Wire Test 675 °C
<br>@Thickness 0.750 mm
1250 °F
<br>@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
675 °C
<br>@Thickness 1.50 mm
1250 °F
<br>@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
675 °C
<br>@Thickness 3.00 mm
1250 °F
<br>@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
700 °C
<br>@Thickness 0.750 mm
1290 °F
<br>@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
700 °C
<br>@Thickness 1.50 mm
1290 °F
<br>@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
700 °C
<br>@Thickness 3.00 mm
1290 °F
<br>@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
<br>@Thickness 0.750 mm
1.00e+13 ohm-cm
<br>@Thickness 0.0295 in
IEC 60093
Dielectric Strength 20.0 kV/mm
<br>@Thickness 1.00 mm
508 kV/in
<br>@Thickness 0.0394 in
IEC 60243
Arc Resistance 60 - 119 sec
<br>@Thickness 3.00 mm
60 - 119 sec
<br>@Thickness 0.118 in
ASTM D495
Comparative Tracking Index 250 - 399 V
<br>@Thickness 3.00 mm
250 - 399 V
<br>@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 14 sec
<br>@Thickness 0.750 mm
7.0 - 14 sec
<br>@Thickness 0.0295 in
UL 746
7.0 - 14 sec
<br>@Thickness 3.00 mm
7.0 - 14 sec
<br>@Thickness 0.118 in
UL 746
15 - 29 sec
<br>@Thickness 1.50 mm
15 - 29 sec
<br>@Thickness 0.0591 in
UL 746
High Amp Arc Ignition, HAI >= 120 arcs
<br>@Thickness 0.750 mm
>= 120 arcs
<br>@Thickness 0.0295 in
UL 746
>= 120 arcs
<br>@Thickness 1.50 mm
>= 120 arcs
<br>@Thickness 0.0591 in
UL 746
>= 120 arcs
<br>@Thickness 3.00 mm
>= 120 arcs
<br>@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Nozzle Temperature 280 - 310 °C
536 - 590 °F
Melt Temperature 285 - 305 °C
545 - 581 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Suggested Max Regrind 25 %