Processing Properties Metric English Comments
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow
Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Rear Barrel Temperature 290 - 310 °C
554 - 590 °F
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Rear Barrel Temperature 282 - 310 °C
540 - 590 °F
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized &n
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
LTL Color Compounds ColorFast® PC60 Polycarbonate
6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled
High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 282 - 310 °C
540 - 590 °F
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Rear Barrel Temperature 282 - 310 °C
540 - 590 °F
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Rear Barrel Temperature 282 - 310 °C
540 - 590 °F
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Rear Barrel Temperature 293 - 310 °C
560 - 590 °F
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 293 - 310 °C
560 - 590 °F
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM
Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Copyright © lookpolymers.com All Rights Reserved