Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 5.23 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools...
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A HSX (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXM3729 PC (Europe-Africa-Middle East)
LEXAN FXM3729 is an UV stabilized Visual FX Sparkle grade, with an excellent flow. It contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
PolyOne Bergamid™ B700 X2 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 49 GF 30 LW PP, 30% glass fibre, coupling agents, laser writer
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties and contains modificator for laser labeling of fini..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 6 LI/1 Polyamide 6, Impacted
FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYabs F20 ABS
Information provided by Polykemi AB
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Styrolution Luran® S KR 2859 UV ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® M210TF ABS
Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber
SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber
Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Suzhou Hipro Polymers Hiprolon® 400 NN Nylon, conditioned
Hiprolon® 400 NN is a medium viscosity specialty polyamide. Features: low density, low water absorption, high dimension stability, high notched impact resistance in large temperature ranges, and..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding
Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This ..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced
Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polyram PlusTek PA310G8BK10 Nylon 6.6 for injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 40% Glass fiber reinforced Nylon 6.6 for injection molding applications. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram.
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30
30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30
30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
DSM EcoPaXX® Q-HG6 PA410-GF30
30% Glass Reinforced, Heat Stabilized
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the..