| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 GB 20 LS PA66, 20% glass beads, light stability
FeaturesPA 66 for injection moulding, chemically reinforced with 20 % glass beads, light stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and elect..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength
FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 GF 15 T 25 PA66, 15% glass fibre, 25% talc
FeaturesChemically reinforced with 15% glass fibre and talc, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical in..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Radici Radilon® A HSX (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Radici Radilon® A RV250 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® S223-G8U (Cond.) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 260 °C | 500 °F | Dry; ISO 11357-3 |
|
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Conditioned)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
|
|||
| Melting Point | 260 - 265 °C | 500 - 509 °F | |
|
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66
Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® MRGF25/25 22H-NBK1 Nylon 66, 25% Mineral and 25% Glass Reinforced
All information provided by Wellman Engineered Resins.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® XT1816-BK1 Toughened Nylon 66
Description: Toughened Nylon 66Information provided by Wellman.
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® S223-HM8 (Dry) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® AS V0 PA66
Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20
Information provided by EMS Grivory
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSS PA666
Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSS/2 FA PA666
Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow ..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSZ 3 PA666
Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug..
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM
15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® 21MST Nylon 66
Vydyne® 21MST is a neat PA66 resin that is designed for extrusion-compounding applications. This general-purpose resin provides excellent viscosity stability against moisture through the extrusion ..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF
Information provided by EMS Grivory
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Radici Radilon® A HSK (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||