Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 285 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 285 - 304 °C
545 - 580 °F
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Melt Temperature 285 - 304 °C
545 - 580 °F
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced
Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66  (Unverified Data**)
Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati..
Melt Temperature 285 - 300 °C
545 - 572 °F
ISO 294
Gromax BTE65-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Melt Temperature 285 °C
545 °F
DAM; Optimum; Extrusion
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Melt Temperature 285 °C
545 °F
DAM; Optimum; Injection Molding
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Melt Temperature 285 °C
545 °F
DAM; Optimum; Injection Molding
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66
Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Melt Temperature 285 °C
545 °F
DAM; Optimum
DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon  (Unverified Data**)
Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by Du..
Melt Temperature 285 - 300 °C
545 - 572 °F
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM; Blow Molding
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66
Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 300 °C
545 - 572 °F
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..