Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 581 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 135 - 305 °C
275 - 581 °F
Average value: 211 °C Grade Count:16
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Melt Temperature 150 - 305 °C
302 - 581 °F
Average value: 212 °C Grade Count:6
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66  (Unverified Data**)
Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po..
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 250 - 305 °C
482 - 581 °F
DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations desi..
Melt Temperature 260 - 305 °C
500 - 581 °F
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin..
Melt Temperature 295 - 305 °C
563 - 581 °F
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 295 - 305 °C
563 - 581 °F
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
Melt Temperature 280 - 305 °C
536 - 581 °F
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry)
Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu..
Melt Temperature 280 - 305 °C
536 - 581 °F
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Conditioned)
Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Melt Temperature 260 - 305 °C
500 - 581 °F
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)<
8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin..