Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Voltage Arc-Tracking Rate, HVTR = 0.398 in/min Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
Average value: 17.8 mm/min Grade Count:3
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746A
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Copyright © lookpolymers.com All Rights Reserved