Processing Properties Metric English Comments
Front Barrel Temperature 293 - 310 °C
560 - 590 °F
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Front Barrel Temperature 293 - 310 °C
560 - 590 °F
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by ..
Front Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow
Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Front Barrel Temperature 293 - 310 °C
560 - 590 °F
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Front Barrel Temperature 288 - 310 °C
550 - 590 °F
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Injection Molding
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov..
Front Barrel Temperature 270 - 310 °C
518 - 590 °F
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant
Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM
Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded
Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Front Barrel Temperature 271 - 310 °C
520 - 590 °F
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..