Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 280 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY
Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY
Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY
Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl..
Front Barrel Temperature 280 - 295 °C
536 - 563 °F
Solvay Specialty Polymers Kalix® 2930 HFFR Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2930 HFFR is a bio-sourced polyamide-based material specifically formulated to meet UL 94V2 @ 0.4 mm requirements for electronic devices. The material uses an advanced halogen-free flame r..
Front Barrel Temperature 280 °C
536 °F
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Front Barrel Temperature 280 - 300 °C
536 - 572 °F
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Front Barrel Temperature 280 - 300 °C
536 - 572 °F
Samyang Trirex® 3500G30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY
Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Front Barrel Temperature 280 - 300 °C
536 - 572 °F
Zone 3
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded
Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Front Barrel Temperature 280 °C
536 °F
Beijing Chemical Industry KAIFA® M106N MPPO Resin
High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay Technyl® A 402 H1 Nylon 66
Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit..
Copyright © lookpolymers.com All Rights Reserved