Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 15 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
UL 746
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose
Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=2.00 mm
15 - 30 sec

@Thickness >=0.0787 in
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=2.50 mm
15 - 30 sec

@Thickness >=0.0984 in
LG Chemical AF345 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose
Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.30 mm
15 - 30 sec

@Thickness >=0.130 in
LG Chemical Lupox® GP1000SB PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=2.00 mm
15 - 30 sec

@Thickness >=0.0787 in
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin
Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=2.00 mm
15 - 30 sec

@Thickness >=0.0787 in
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
All colors
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 0.750 mm
15 - 30 sec

@Thickness 0.0295 in
PLC 3
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746A
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 3.00 mm
15 - 29 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 3.00 mm
15 - 29 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 3.00 mm
15 - 30 sec

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 3.00 mm
15 - 29 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
UL 746A
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Hot Wire Ignition, HWI 15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Copyright © lookpolymers.com All Rights Reserved