| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
| Ineos ABS Triax® 3158 ABS + Polyamide Blend (DAM), PA66/ABS Pellets (filled) Triax® 3158 is a PA+ABS-Blend and on-line paintable (195°C). It has very high heat resistance, reduced moisture, improved impact strength, and a low coefficient of linear thermal expansion. It.. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
| Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature -40.0 °C |
<= 4.76 ft-lb/in² @Temperature -40.0 °F |
d.a.m.; ISO 180-1A |
| Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1A |
| Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1A |
| Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
| Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
| Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1A |
| Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1A |
| Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | <= 10.0 kJ/m² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
| Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1A |
| Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180-A |
| Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
| Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 179/1eA |
| Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180-A |
| Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
| Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Eurotec® Tecomid® NB40 GR30 NL AX70 PA6, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
| Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
| Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
| Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
| Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
| Izod Impact, Notched (ISO) | 10.0 kJ/m² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
| DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |
|||