Polymer Property : Mold Temperature = 95.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
temperatures as low as 10°C (50°F) can be used where applicable.
BASF Capron® 8203C Nylon 6 (Conditioned)  (discontinued **)
Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate
Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy
Information provided by A. Schulman.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman ComAlloy® E-12672 Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy
Information provided by A. Schulman.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy
Information provided by A. Schulman.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy
Information provided by A. Schulman.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy
Information provided by A. Schulman.
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded
Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded
Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance..
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry)
Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the..
Mold Temperature 15.0 - 95.0 °C
59.0 - 203 °F
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Mold Temperature 30.0 - 95.0 °C
86.0 - 203 °F
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..