| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow
Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow
Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
PLC 0 |
|
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 2.00 mm
|
>=
120
arcs <br>@Thickness 0.0787 in
|
|
|
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
|
|
LG Chemical AF345 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 6.00 mm
|
>=
120
arcs <br>@Thickness 0.236 in
|
|
|
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
|
|
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
|
|
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
|
|
LG Chemical Lupox® GP2100 PBT+GF10%
Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.60 mm
|
>=
120
arcs <br>@Thickness 0.0630 in
|
|
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 2.00 mm
|
>=
120
arcs <br>@Thickness 0.0787 in
|
|
|
LG Chemical LUPOL GP3156F Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided ..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.60 mm
|
>=
120
arcs <br>@Thickness 0.0630 in
|
|
|
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 2.50 mm
|
>=
120
arcs <br>@Thickness 0.0984 in
|
|
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical LUPOY GP1000M PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
|
|
LG Chemical XR404 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
All colors |
|
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
All colors; PLC 0 |
|
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded
Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 0.750 mm
|
>=
120
arcs <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 3.00 mm
|
>=
120
arcs <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 0.710 mm
|
>=
120
arcs <br>@Thickness 0.0280 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.50 mm
|
>=
120
arcs <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| High Amp Arc Ignition, HAI |
>=
120
arcs <br>@Thickness 1.60 mm
|
>=
120
arcs <br>@Thickness 0.0630 in
|
|
|
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
|
|||