| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.710 mm |
7.0 - 14 sec @Thickness 0.0280 in |
UL 746 |
| Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746A |
| Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.710 mm |
7.0 - 14 sec @Thickness 0.0280 in |
UL 746 |
| Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
| Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
| Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
| Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
| Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.710 mm |
7.0 - 14 sec @Thickness 0.0280 in |
UL 746 |
| Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||