| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | Crystalline Density; ASTM D1505 |
|
Eastman Aqua 18696 PET
(discontinued **)
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® SC699 NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® SC699 is a low viscosity acetal homopolymer, lubricated, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D790 |
|
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
|
|||
| Density |
1.40
g/cc @Temperature 23.0 °C |
0.0506
lb/in³ @Temperature 73.4 °F |
ASTM D1505-68, method C |
|
Mitsubishi Hostaphan® RN, 75 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Xenoy® XD1607 PBT+PC (Europe-Africa-Middle East)
22% Glass filled PBT+PC with a designed balance between surface appearance and mechanical properties sufficient for automotive doorhandle requirements. Special suitable for gas assist mouldings .Thi..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as ..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
Chengdu Polyster FH4543 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H4543 and self-made flame retardant material. Flame retardant, good balance of low and high temperature properties. Applications requiring flame retardancy, such as wires, cables and optica..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
|
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | Average value for Mylar® films. |
|
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | Average value for Mylar® films. |
|
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | cured 14 days @ 50% RH |
|
3M AC-350 Class A-1 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
BASF LUMOGEN® 300 F Red
Type of Dye: PeryleneNote on Fastness to Weathering: 0.02% in PMMA injection-molded plaques of 2 mm thickness Residual fluorescence(%) after 80 days accelerated exposure in Xenotest 1200Information ..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
|
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
|
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | Average value for Mylar® films. |
|
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated
(discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific)
LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber.
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
|
Plenco 7579 Phenolic, Granular, Compression Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | Liquid |
|
3M Novec™ 7000 Engineered Fluid
3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a..
|
|||
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
|
Polyplastics Duracon® M270-48 Acetal Co-polymer (POM), Antistatic, High flow
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Density |
1.40
g/cc @Temperature 23.0 °C |
0.0506
lb/in³ @Temperature 73.4 °F |
ASTM D792 |
|
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||