| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 123 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 940ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746 |
|
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® HP1R PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | |
|
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
|
|||
| Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
|
Mitsubishi Xantar® 19 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Comparative Tracking Index | 250 V | 250 V | d.a.m.; Solution A; IEC 60112 |
|
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS.
|
|||
| Comparative Tracking Index | 250 V | 250 V | A solution |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin ..
|
|||
| Comparative Tracking Index | 250 V | 250 V | A solution |
|
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin
Polycarbonate-resin-base flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even at a thinner th..
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
Information provided by PolyPlastics.
|
|||
| Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
|
Toyobo VYLOPET® EMC407 Non-Reinforced
Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessImproved processabilityHigh fluidityGood appearanceInformation provided by Toyobo.
|
|||
| Comparative Tracking Index |
250
V @Thickness 3.00 mm |
250
V @Thickness 0.118 in |
IEC 60112; IEC/EN 60893-2 6.4 |
|
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
|
|||
| Comparative Tracking Index | 250 V | 250 V | Solution A; IEC 60112 |
|
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
Covestro Makrolon® LTG2623 Polycarbonate
PreprocessingMax. Water content
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
|
Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Comparative Tracking Index |
250
-
399
V @Thickness 3.00 mm |
250
-
399
V @Thickness 0.118 in |
IEC 60112 |
|
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Comparative Tracking Index | 250 V | 250 V | Test solution A; IEC 112 |
|
BASF Ultradur® B 4406 PBT
Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo..
|
|||
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
|
SABIC Innovative Plastics Lexan® 103R PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release...
|
|||
| Comparative Tracking Index | 250 V | 250 V | Test solution A; IEC 112 |
|
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT
Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila..
|
|||
| Comparative Tracking Index | 250 V | 250 V | A solution |
|
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri..
|
|||